Mechanical Properties Metric English Comments
Modulus of Elasticity 0.330 - 2.07 GPa
47.9 - 300 ksi
Average value: 1.22 GPa Grade Count:10
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Modulus of Elasticity 0.330 GPa
47.9 ksi
Molded Sample 2% Secant Modulus
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and..