Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00268 GPa | 0.388 ksi | After 7 days at 100°C; ASTM D412 ISO 37 |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |