Mechanical Properties Metric English Comments
Modulus of Elasticity 0.442 GPa
64.1 ksi
Secant; ASTM D638
Huntsman PE1080 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under..