Polymer Property : Modulus of Elasticity = 0.488 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00336 GPa
0.488 ksi
ASTM D638
Colorite Polymers Elastichem 6011TX-02 Vinyl Compound
Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co..