Polymer Property : Modulus of Elasticity = 0.537 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00370 - 215 GPa
0.537 - 31200 ksi
Average value: 35.9 GPa Grade Count:99
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..