Polymer Property : Modulus of Elasticity = 0.552 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.552 GPa
80.1 ksi
Molded Sample 2% Secant Modulus
Dow DOWLEX™ IP-22 High Density Polyethylene
DOWLEX® IP-22 resin is an improved processing high density polyethylene resin designed for excellent flow, high impact, and moderate stiffness. DOWLEX IP-22 resin balances peak molecular weight wit..