Mechanical Properties Metric English Comments
Modulus of Elasticity 0.793 GPa
115 ksi
Plastic Lumber from the Plastic Lumber Co.
Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep..