Polymer Property : Modulus of Elasticity = 1.227 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.227 - 1.462 GPa
178.0 - 212.0 ksi
ASTM D638M
DSM Somos® 9120 Epoxy Photopolymer  (Unverified Data**)
DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p..
Modulus of Elasticity 1.227 - 1.462 GPa
178.0 - 212.0 ksi
UV Postcure; ASTM D368M
DSM Somos® 9120
The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp..