Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.009894 GPa | 1.435 ksi | Calculated; ASTM D412 Method A |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |