Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.76 GPa | 255 ksi | ASTM D-638 |
Plaskolite Optix® CA - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 1.76 GPa | 255 ksi | ASTM D-638 |
Plaskolite Optix® CA - 1000 E-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 1.76 GPa | 255 ksi | ASTM D-638 |
Plaskolite Optix® CP - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Modulus of Elasticity | 1.76 GPa | 255 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 1.76 GPa | 255 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 1.76 GPa | 255 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Modulus of Elasticity | 1.76 - 3.65 GPa | 255 - 530 ksi | Average value: 2.86 GPa Grade Count:124 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 1.76 - 10.7 GPa | 256 - 1550 ksi | Average value: 6.74 GPa Grade Count:18 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |