Mechanical Properties Metric English Comments
Modulus of Elasticity 1.793 GPa
260.1 ksi
ASTM D638
Ineos Nova 5420 High Impact Polystyrene  (discontinued **)
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m..