Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.965 GPa | 285.0 ksi | ASTM D638 |
Ineos Nova 5540 High Impact Polystyrene
(discontinued **) Excellent balance of toughness, flow, and set-up, High gloss, USP Class VIApplications: Structural foam, Housewares, Toys, Appliance parts, Dairy containersProperties were determined on injection mo.. |