Mechanical Properties Metric English Comments
Modulus of Elasticity 0.074980 GPa
10.875 ksi
Humiseal 2A64 Urethane Conformal Coating
Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F..