Polymer Property : Modulus of Elasticity = 106 ksi
Polymer Property :
Modulus of Elasticity =
106 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Modulus of Elasticity
0.730
GPa
106
ksi
Reliance Industries BIOMER P240
compared to LDPE, HDPE, PHBInformation provided by Reliance Industries