Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 73.6 GPa | 10700 ksi | |
Mateck Fused Silica IR Grade (SiO2) Optical crystals |
|||
Modulus of Elasticity | 73.6 GPa | 10700 ksi | |
Mateck Fused Silica UV-VIS Grade (SiO2) Optical crystals |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Schott N-PK51 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Modulus of Elasticity | 74.0 GPa | 10700 ksi | |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Vista Metals Duramold-2™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 400 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 600 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 500 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Modulus of Elasticity | 73.8 GPa | 10700 ksi | |
Aleris Weldural Aluminum Alloy, 700 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |