Mechanical Properties Metric English Comments
Modulus of Elasticity 75.8 GPa
11000 ksi
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite
Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem..
Modulus of Elasticity >= 76.0 GPa

@Temperature 200 °C
>= 11000 ksi

@Temperature 392 °F
Condition T6x (Quench in water at RT)
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Modulus of Elasticity >= 76.0 GPa

@Temperature 200 °C
>= 11000 ksi

@Temperature 392 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
Modulus of Elasticity 76.0 GPa
11000 ksi
Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance ..
Modulus of Elasticity 76.0 GPa
11000 ksi
Piezo Kinetics 409E Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance ..
Modulus of Elasticity 76.0 GPa
11000 ksi
Schott LITHOTEC-CAF2 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 76.0 GPa
11000 ksi
Schott N-PSK53A Glass
Information Provided by SCHOTT North America, Inc.