Polymer Property : Modulus of Elasticity = 113 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.490 - 0.780 GPa
71.1 - 113 ksi
ASTM D638
Zeus EFEP Tubing
Modulus of Elasticity 0.490 - 0.780 GPa
71.1 - 113 ksi
ASTM D638
Zeus ETFE Tubing
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess..