Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.10 - 8.64 GPa | 595 - 1250 ksi | Average value: 7.00 GPa Grade Count:5 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |