Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 8.69 - 13.0 GPa | 1260 - 1890 ksi | Average value: 10.5 GPa Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 8.70 - 10.1 GPa | 1260 - 1460 ksi | Average value: 9.43 GPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Modulus of Elasticity | 8.70 GPa | 1260 ksi | ISO 527-2 |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connect.. |