Mechanical Properties Metric English Comments
Modulus of Elasticity 89.0 GPa
12900 ksi
Young's Modulus
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite
Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate..
Modulus of Elasticity 89.0 GPa
12900 ksi
Young's Modulus
MMCC Copper/Graphite Fiber GC 7-340 Metal Matrix Composite
Discontinuous graphite fiber copper product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plated,..
Modulus of Elasticity 89.0 GPa
12900 ksi
Schott N-BAF10 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 89.0 GPa
12900 ksi
Schott N-SK16 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 89.0 GPa
12900 ksi
Schott N-KZFS5 Glass
Information Provided by SCHOTT North America, Inc.