Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 130 GPa @Temperature 1000 °C |
18900 ksi @Temperature 1830 °F |
|
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Modulus of Elasticity | 130 GPa | 18900 ksi | |
CLAL-MSX NICLAL 1300 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Modulus of Elasticity | 130 GPa | 18900 ksi | |
CLAL-MSX NICLAL 1800 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Modulus of Elasticity | 130 GPa | 18900 ksi | |
CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Modulus of Elasticity | 130 GPa | 18900 ksi | |
CLAL-MSX NICLAL 1800 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Modulus of Elasticity | 130 GPa | 18900 ksi | longitudinal |
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Modulus of Elasticity | 130 GPa | 18900 ksi | |
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Modulus of Elasticity | 130 GPa @Temperature 800 °C |
18900 ksi @Temperature 1470 °F |
|
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Modulus of Elasticity | 130 GPa @Temperature 800 °C |
18900 ksi @Temperature 1470 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |