Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Pacific Sintered Materials F-240-S(HT) Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-60(HT)All information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 245C Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Strip; A -Dead Soft (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy M25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy M25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Schmolz + Bickenbach MoldMAX HH® High Hard - Copper Alloy Description: Brush Wellman’s MoldMAX HH® (High Hard) is the premier copper mold alloy. This alloy has a hardness and strength comparable with standard tool steels but its thermal conductivit.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |
|||
Modulus of Elasticity | 131 GPa | 19000 ksi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its .. |