Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.80 - 11.6 GPa @Temperature -40.0 - 150 °C |
696 - 1680 ksi @Temperature -40.0 - 302 °F |
Average value: 7.45 GPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Modulus of Elasticity | 8.40 - 11.6 GPa | 1220 - 1680 ksi | Average value: 9.93 GPa Grade Count:15 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |