Mechanical Properties Metric English Comments
Modulus of Elasticity 0.720 - 1.19 GPa
104 - 172 ksi
Average value: 0.936 GPa Grade Count:3
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..