Mechanical Properties Metric English Comments
Modulus of Elasticity 119 GPa

@Temperature 982 °C
17300 ksi

@Temperature 1800 °F
Carlson C 825 Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st..
Modulus of Elasticity 119 GPa
17300 ksi
Trans.
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Modulus of Elasticity 119 GPa
17300 ksi
Long.
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..