Mechanical Properties Metric English Comments
Modulus of Elasticity 122 GPa
17700 ksi
Wieland Simidur S 2 PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Modulus of Elasticity 122 GPa
17700 ksi
In rolling direction
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Modulus of Elasticity 122 GPa
17700 ksi
In rolling direction
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Modulus of Elasticity 122 GPa
17700 ksi
In rolling direction
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Modulus of Elasticity 122 GPa
17700 ksi
In rolling direction
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..