Modulus of Elasticity 1.25 GPa
181 ksi
ISO R527
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Modulus of Elasticity 1.25 GPa
181 ksi
ISO 178
Addiplast Addilene H 210 Polypropylene Homopolymer
UnreinforcedInformation provided by Addiplast.