Polymer Property : Modulus of Elasticity = 184 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.27 GPa
184 ksi
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon
The integration of 25% carbon increases the wear resistance, hardness, and creep strength of this material. Murflor® + Carbon is used, for example, when electrical conductivity is required and Mate..
Modulus of Elasticity 1.27 - 1.27 GPa

@Temperature 80.0 - 80.0 °C
184 - 184 ksi

@Temperature 176 - 176 °F
Average value: 1.27 GPa Grade Count:1
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..