Polymer Property : Modulus of Elasticity = 1870 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 12.9 GPa
1870 ksi
ASTM C580
Chesterton ARC 791 Composite
Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex..