Mechanical Properties Metric English Comments
Modulus of Elasticity 4.00 - 19.788 GPa

@Temperature -40.0 - 200 °C
580 - 2870.0 ksi

@Temperature -40.0 - 392 °F
Average value: 8.59 GPa Grade Count:9
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..