Mechanical Properties Metric English Comments
Modulus of Elasticity 2.392 GPa
346.9 ksi
Kleerdex Kydex® 115 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
High rigidity sheet for ceiling panelsApplications: Ceiling panels in clean rooms, computer rooms, laboratories, food, dairy, and pharmaceutical plants, and other environments where a high degree of..