Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.517 GPa | 365.1 ksi | |
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may.. |