Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.96 GPa | 429 ksi | ASTM D638 |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Modulus of Elasticity | 2.96 - 55.8 GPa | 430 - 8090 ksi | Average value: 21.3 GPa Grade Count:19 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 2.96 - 11.7 GPa | 430 - 1700 ksi | Average value: 6.71 GPa Grade Count:14 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |