Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.00 - 138 GPa | 145 - 20000 ksi | Average value: 22.1 GPa Grade Count:181 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |