Mechanical Properties Metric English Comments
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 0% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 1000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 4000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa

@Temperature 300 °C
30300 ksi

@Temperature 572 °F
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Modulus of Elasticity 209 GPa
30300 ksi
Dynamic
Special Metals INCONEL® alloy 22 Austenitic Alloy
INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat..
Modulus of Elasticity 209 GPa
30300 ksi
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
An oil-hardening alloy with excellent size change properties, Stentor tool steel is especially suited for general purpose work in the toolroom. It is safe to harden, and shows little size change or ..