Mechanical Properties Metric English Comments
Modulus of Elasticity 21.6 GPa
3130 ksi
ASMT D638
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..