Polymer Property : Modulus of Elasticity = 21.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.150 GPa
21.8 ksi
ISO 527-2
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grindin..
Modulus of Elasticity 0.150 GPa
21.8 ksi
Molded Sample 2% Secant Modulus
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f..
Modulus of Elasticity 0.150 GPa
21.8 ksi
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Copyright © lookpolymers.com All Rights Reserved