Polymer Property : Modulus of Elasticity = 2100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 14.5 GPa
2100 ksi
Poco Graphite ZXF-5Q Industrial Grade Graphite
SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p..
Modulus of Elasticity 14.5 GPa
2100 ksi
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Modulus of Elasticity 14.5 GPa
2100 ksi
IPC TM-650 2.4.18.3
Arlon 38N High Performance Polyimide Low-Flow
38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow..
Modulus of Elasticity 14.5 GPa
2100 ksi
ISO 178
Addiplast Addinyl B2 V50 Nylon 6, 50% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 14.5 GPa
2100 ksi
ISO 178
Addiplast Addinyl B2 ZV 50 Nylon 6, 50% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 14.5 GPa
2100 ksi
DIN 53 457
Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber
High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Impellers, Valve Housings and BushingsProcessing: Injection Molding (..
Modulus of Elasticity 14.5 GPa
2100 ksi
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..