Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 216 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 216 GPa
31300 ksi
Poco Graphite SUPERSiC® 3C Silicon Carbide
SUPERSiC that has been coated with a 75 µm CVD SiC coating, which seals the surface.Uses: Ideal for high-temperature deposition and CVD applications.Information provided by PocoGraphite
Modulus of Elasticity 216 GPa
31300 ksi
Poco Graphite SUPERSiC® 3CX Silicon Carbide
SUPERSiC that has been coated twice with a 75 µm CVD SiC coating, which seals the surface. Uses: Ideal for high-temperature anneal processesInformation provided by PocoGraphite
Modulus of Elasticity 216 GPa
31300 ksi
Poco Graphite SUPERSiC® Basic Silicon Carbide
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 216 GPa
31300 ksi
RT
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..