Polymer Property : Modulus of Elasticity = 220.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 220.6 GPa
31990 ksi
Latrobe Lescalloy® BG42 VIM-VAR High Performance Bearing Steel
LESCALLOY BG42 VIM-VAR steel is a martensitic, stainless high speed steel that combines the tempering, hot hardness and hardness retention characteristics of M50 high speed steel with the corrosion ..