Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 2200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 10.3 - 15.2 GPa
1500 - 2200 ksi
Average value: 13.0 GPa Grade Count:6
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Modulus of Elasticity 2.75 - 15.2 GPa
399 - 2200 ksi
Average value: 8.65 GPa Grade Count:31
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
Modulus of Elasticity 2.76 - 15.2 GPa
400 - 2200 ksi
Average value: 6.95 GPa Grade Count:59
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Modulus of Elasticity 3.10 - 15.2 GPa
450 - 2200 ksi
Average value: 5.35 GPa Grade Count:33
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved