Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 15.5 - 19.0 GPa | 2250 - 2760 ksi | Average value: 17.0 GPa Grade Count:11 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Modulus of Elasticity | 15.5 GPa | 2250 ksi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |