Polymer Property : Modulus of Elasticity = 228 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 228 GPa
33100 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4 Carbon Fiber (12,000 Filaments)
Weight/length = 0.858 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 228 GPa
33100 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4 Carbon Fiber (3000 Filaments)
Weight/length = 0.210 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 228 GPa
33100 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4 Carbon Fiber (6000 Filaments)
Weight/length = 0.427 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 228 GPa
33000 ksi
(hardened and tempered)
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh..