Polymer Property : Modulus of Elasticity = 240 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 220 - 240 GPa
31900 - 34800 ksi
Youngs Modulus
MMCC Cu/Al2O3 Particulate Copper Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).