Mechanical Properties Metric English Comments
Modulus of Elasticity 1.862 GPa
270.1 ksi
ASTM D638
Ineos Nova 5500 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..
Modulus of Elasticity 1.862 GPa
270.1 ksi
ASTM D638
Ineos Nova 5504 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..