Mechanical Properties Metric English Comments
Modulus of Elasticity 16.0 - 20.0 GPa
2320 - 2900 ksi
Injection; ISO 527
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Modulus of Elasticity 5.86 - 20.0 GPa
850 - 2900 ksi
Average value: 11.6 GPa Grade Count:36
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Modulus of Elasticity 4.10 - 20.0 GPa
595 - 2900 ksi
Average value: 14.3 GPa Grade Count:24
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..