Mechanical Properties Metric English Comments
Modulus of Elasticity 0.280 - 2.05 GPa
40.6 - 297 ksi
Average value: 0.710 GPa Grade Count:12
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..