Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.52 GPa | 510 ksi | ASTM D638 |
Radici Radilon® N66-AFR Nylon 66
(discontinued **) |
|||
Modulus of Elasticity | 3.52 GPa | 511 ksi | ASTM D638M |
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |
|||
Modulus of Elasticity | 3.52 GPa | 510 ksi | Machine; ASTM D638 |
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin.. |