Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.75 GPa | 544 ksi | ISO 527 |
DSM Fibre Intermediates Nyrim® 1525 (Glass), Dry Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Modulus of Elasticity | 3.75 GPa @Temperature 40.0 °C |
544 ksi @Temperature 104 °F |
ISO 527 |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |