Polymer Property : Modulus of Elasticity = 3.77 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0260 GPa
3.77 ksi
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Modulus of Elasticity 0.0260 GPa
3.77 ksi
ASTM D412
KKPC KOSYN KTR 402 Thermoplastic Elastomer (TPE)
Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics ..